Hello, 

great to have a forum like this. Thumbs up!

I am looking at creating a carbon fiber copy of my motorcycle dash. 

I do have some questions regarding the method connected to this, but first of all I was wondering if I'm good off with an Epoxy Mould Making Starter Kit, together with a Carbon Fibre Laminating Starter Kit. Will I have enough material to make a copy of this dash? 

http://storage1.colony1.net/2195/Product_Photos/6-23-10%20031.jpg


Thank you!

Yours sincerely
Nat
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
PM sent

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search