Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I agree with Warren, flat sheet is easiest option and likely to yeild best results for a novice. Wet lay is perfectly possible but will take practice to make a good one. Out of Autoclave pre-preg would be good too but not a cheap option!
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|