Hello All,

Does anybody knows how to disperse SiC fibers in ceramic slurry?

thanks in advanced
Reply
compositepro
compositepro
Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)Supreme Being (242 reputation)
Group: Forum Members
Posts: 22, Visits: 65
Sorry chief cant really help you on that one then 

Its a broad ranger im afraid and my experience is that of ceramic exhaust systems

what kind of milling process are you using 

vacuum infiltration is most common, though vibration can also be considered followed by HIP 