Hello All,
Does anybody knows how to disperse SiC fibers in ceramic slurry?
thanks in advanced
By compositepro
-
7/14/2013 7:44:58 PM
Sorry chief cant really help you on that one then
Its a broad ranger im afraid and my experience is that of ceramic exhaust systems
what kind of milling process are you using
vacuum infiltration is most common, though vibration can also be considered followed by HIP