Back in 2011 I purchased a range of equipment from EC and up until now I was using the resin catchpot as a vacuum chamber to degas my resin because it came as part of the resin infusion kit.

But even with the admittedly small quantity of resin I have been needing to degas recently (maybe 15g resin plus half qty hardener) I was finding that it would reach the top of a pint cup inside my makeshift vacuum chamber aka resin catchpot and need alot of cleaning up.

So, rather than get the huge 26+ litre EC degassing chamber I've decided to take a punt on the vac-it-pro 3 gallon vacuum chamber from the USA.

I will provide an update once I receive it but youtube videos from users of the product seem positive and the design seems nice.  I first came across it when a youtube user meganbeads has a video degassing resin, admittedly a different type of resin to what we are using but the vac chamber itself does the job.
Reply
FiftyPence
FiftyPence
Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)Supreme Being (194 reputation)
Group: Forum Members
Posts: 26, Visits: 264
Received the vac-it-pro 3 gallon vacuum chamber today and it works perfectly.  A very nice piece of kit and very cost effective (~£140) compared to anything I could find in the UK (>£250).