Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Dual vacuum pumps?
Dual vacuum pumps?
Post Reply
Like
2
Dual vacuum pumps?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 243,
Visits: 1K
I have 2 vacuum pumps. I was wondering if having both working at the same time will be of any advantage.
I would either put 2 valves on the bag, or hook up both pumps to a manifold and have a hose go from the manifold to the bag.
My question is: Will the total vacuum pull be stronger, or will the pumps fight against each other?
Reply
Like
2
Reply
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
One is a generic chinese pump, same as the EC one, the other is an Alcatel heavy duty one.
I did notice it sucks the air quicker, but I was wondering what it would do in terms of debulking or leaving them running while the part is cooking.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Dual vacuum pumps?
carboncactus
-
12 Years Ago
My thinking is it will pull the bag down quicker as there is a bigger volume being sucked out but i...
Daz
-
12 Years Ago
I'm thinking the same as Daz... Easy composites pumps already go real far in vacuum
matthieutje65
-
12 Years Ago
All it will do is suck the air out quicker. One pump will work slightly harder than the other as...
Warren (Staff)
-
12 Years Ago
One is a generic chinese pump, same as the EC one, the other is an Alcatel heavy duty one. I did...
carboncactus
-
12 Years Ago
theyd both be off load and just sit there doing very little. Assuming you have a sealed bag that is....
Warren (Staff)
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search