By carboncactus - 6/5/2013 2:29:20 PM

I have 2 vacuum pumps. I was wondering if having both working at the same time will be of any advantage.
I would either put 2 valves on the bag, or hook up both pumps to a manifold and have a hose go from the manifold to the bag.

My question is: Will the total vacuum pull be stronger, or will the pumps fight against each other?
By Warren (Staff) - 6/6/2013 3:40:55 PM

theyd both be off load and just sit there doing very little. Assuming you have a sealed bag that is.