Not sure is this is the right area to post. I have a carbon fibre part that has partial decals applied to it and then was clear coated.

If there a method/Technique anyone knows about that will allow me to remove the clear coat and decals?

I will probably re-apply some clear coat afterwards.

Thanks in advance.

N
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Only way to go is to very carefully sand down the decals and then sand the entire surface very lightly, then apply new clear coat... make sure you get a nice even and smooth surface, an be careful not to sand down into the CF weave.

Good luck..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search