By nutz - 6/3/2013 8:42:18 AM

Hi All,

Not sure is this is the right area to post. I have a carbon fibre part that has partial decals applied to it and then was clear coated.

If there a method/Technique anyone knows about that will allow me to remove the clear coat and decals?

I will probably re-apply some clear coat afterwards.

Thanks in advance.

N
By Dravis - 6/3/2013 2:51:45 PM

Only way to go is to very carefully sand down the decals and then sand the entire surface very lightly, then apply new clear coat... make sure you get a nice even and smooth surface, an be careful not to sand down into the CF weave.