hi im new to these forums and fairly new to the various carbon manufacturing processes. Im sure this question has been asked before or its so plainly obvious that it has not. i am just wondering are you able to put the vacuum pump into the oven itself when making your prepreg parts. and if you are not able to how would u ensure that the vacuum tubing is not blocked off. this is in a non autoclave situation!
Reply
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Hole in the oven and silicone hoses:



Give these guys a ring, they supply big names like TygaVac.

http://www.hosetechnologies.com/aerospace-product.php?c=91&p=237

Depends on how much you buy though, I think they will charge like £15 shipping. If you only need a metre or so, I've got some here you can buy off me.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search