For ease of use id go with the 40mm because its easier to contract braided sleeve than it is to expand it.
However, if you are looking for ultimate strength and an even fibre distribution, i would go for 20mm as expended to 21mm the fibre angle will be closer to 45 degrees so better for a more even tube construction.