I keep coming across the same problem.

In the final stage of flatting and polishing minute white speckles appear in the epoxy. 

My process, 1 st coat , coating epoxy , 8 > 10 hr cure @ 20*

hand 120 dry sand , brush off dust , vacume.

2nd coat , coating epoxy 8 > 10 hrs cure @ 20*

hand sand wet - 320 > 600 > 1200 > 1500 > 2000

everything looks good at this stage even flat finish no blemishes really, just needs buffing up...

so 

machine polish - ( cheap electric car plisher ) onto wet surface -  farecla standard compound G 3 ( SPECKS APPEAR  Wink> farecla ploshiing compound G10 ( SPECKS REMAIN )

it does not always happen but it doeas happen a lot 

any ideas

Ben
Reply
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
here is a quick video on whotube regarding a homemade degassing chamber, it will all become clear after watching it and you may have things laying around you could use already!

http://www.youtube.com/watch?v=dxVbFwHpg7Q

good luck Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
benet - 12 Years Ago
neilb - 12 Years Ago
fgayford - 12 Years Ago
carboncactus - 12 Years Ago
fgayford - 12 Years Ago
benet - 12 Years Ago
carbonfibreworks - 12 Years Ago
neilb - 12 Years Ago
benet - 12 Years Ago
neilb - 12 Years Ago
benet - 12 Years Ago
neilb - 12 Years Ago
benet - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search