here is a quick video on whotube regarding a homemade degassing chamber, it will all become clear after watching it and you may have things laying around you could use already!

http://www.youtube.com/watch?v=dxVbFwHpg7Q

good luck Smile
benet
benet
Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)Supreme Being (901 reputation)
Group: Forum Members
Posts: 59, Visits: 373
this kind of thing 

fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Yes it is wax and you would not be able to clear on to that. I was just suggesting it if you are as done as you are going to go. Then the black in the wax would hide the tiny pin holes.

Fred   