do you heat the resin before mixing or after?
I can recall fred advising another forum user of a technique to remove air bubbles which involves the resin being pored (when mixed) from a height (around 12-18 inches I think) slowly into another container apparently this causes the air bubbles to pop. worth a try cause its free!
other than that build a degas chamber with some Perspex sheet and tube silicone'd together, make a rubber gasket for the top, piece of Perspex with a small hole in it for the lid and vacuum the air out with a small vacuum cleaner. it just may work!