This is a promotional video, made by an advertising bureau ... They have cut and mixed up their takes from the manufacturing, and are not showing them in the correct sequence.
What looks like resin in one part of the presentation, is in fact 2-comp clear PU coat... put it on very liberally ,and grind and sand and polish it afterwards.
This surface is very resistant to most chemicals (as advertised) and also fire-retardant and can withstand burning a thin coat of alcohol or petroleum on the surface... nothing special in that...
Looks to me like they do most of it as skinning and thick layers of PU coat ... = cosmetic parts "made with genuine Carbon fibre"