Hi all friends
just looked at robson design carbon wrap promo video i dont get why they lay resin on clear tape on top then sand with wet paper and clear coat? any idea?
how carbon surface can not be burned on their parts and why chemical resistance?
https://www.youtube.com/watch?feature=player_embedded&v=Rg7f9EaXpoA
Please look at this video he tape part and seems parts no resin then he lay clear tape and see on video when he lay resin tape clear under resin then only cut and wet sanding and etc.
By TomDesign
-
4/25/2013 9:06:08 AM
ye i tryed polyster resin is nightmare for carbon stuff.
i just discovered superb epoxy resin with carbon fiber to work with. so i hope to post results very soon.