Jayyy88
Jayyy88
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 26
I've recently purchased both the laminating kit and mould making kit. I'm looking to get started today however having watched the YouTube videos I have a few questions before I start.
As its an iPhone 5 case I will be making, when moulding should I consider the slight overlap of plastic when making the mould? Or would it be best to not make a mould and lay the carbon down inside?
I notice in the video the putty is placed around the edges however not all the way to the surface of the plastic work area is this purely to stop mechanical lock? Will I also need to consider the overlap as the case will not snap to the phone when made?
Could anyone give me an idea of the mixture I will need to make the mould as I do not want any waste?
I do not have a plastic work surface can I use a plastic food tray?
Finally I do not have the polishing agent is this necessary in getting a good mould or can an alternative household product suffice?
I hope my questions makes sense.
Reply
Like
3
Reply
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Jayyy88 (31/03/2013)
I've recently purchased both the laminating kit and mould making kit. I'm looking to get started today however having watched the YouTube videos I have a few questions before I start.
As its an iPhone 5 case I will be making, when moulding should I consider the slight overlap of plastic when making the mould? Or would it be best to not make a mould and lay the carbon down inside?
I notice in the video the putty is placed around the edges however not all the way to the surface of the plastic work area is this purely to stop mechanical lock? Will I also need to consider the overlap as the case will not snap to the phone when made?
Could anyone give me an idea of the mixture I will need to make the mould as I do not want any waste?
I do not have a plastic work surface can I use a plastic food tray?
That will work with epoxy not polyester. Tooth paste is a very fine polish.
Finally I do not have the polishing agent is this necessary in getting a good mould or can an alternative household product suffice?
I hope my questions makes sense.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
iPhone 5 case mould
Jayyy88
-
12 Years Ago
Can anyone help?
Jayyy88
-
12 Years Ago
First of all. you want to make not easy stuff. think your parts is rubber? if you do mold you need...
TomDesign
-
12 Years Ago
[quote][b]Jayyy88 (31/03/2013)[/b][hr]I've recently purchased both the laminating kit and mould...
fgayford
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search