i dont get guys i tryed on epoxy wraped part to lay polyster resin it worker surface became hard and great now i used very clear 320 poyster resin and after night in garage in 5+ only it was a little tacky after half of day more in warm home it became more tacky then ever? maybe thats what it needs to dry? as it said that resin needs best to dry +25

i dont get this.
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Not sure why you want to put polyester over epoxy? Why mix the types of resin being used.
( By the way how are you? good I hope.)

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search