Group: Forum Members
Posts: 454,
Visits: 2.5K
|
i dont get guys i tryed on epoxy wraped part to lay polyster resin it worker surface became hard and great now i used very clear 320 poyster resin and after night in garage in 5+ only it was a little tacky after half of day more in warm home it became more tacky then ever? maybe thats what it needs to dry? as it said that resin needs best to dry +25
i dont get this.
|