Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
https://www.easycomposites.co.uk/polyurethane-resin

Hi.

Im looking to remould the plug from my 2 part mould after destroying the original using this casting resin. Problem is (unless im blind) I cant see where it says how much 2kg will fill in volume ? Also it possible to thicken the resin during application as pretty sure if the viscosity is too low it will just flow between the gaps. Finally, should I wax and release agent the moulds before casting ?

Thanks
Reply
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Lol as it being a 2 part mould I had trouble sealing the edges. So i silicone sealed it with my companies normal stuff. Holy s*** its strong, thought i was gonna destroy the mould after I took it apart.

My pattern volume 1250ml so looks like im gnna be buying this product Smile