Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Fast Cast Polyurethane Casting Resin 2kg Pack
Fast Cast Polyurethane Casting Resin 2kg Pack
Post Reply
Like
3
Fast Cast Polyurethane Casting Resin 2kg Pack
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jack.Strong
Jack.Strong
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 52,
Visits: 549
https://www.easycomposites.co.uk/polyurethane-resin
Hi.
Im looking to remould the plug from my 2 part mould after destroying the original using this casting resin. Problem is (unless im blind) I cant see where it says how much 2kg will fill in volume ? Also it possible to thicken the resin during application as pretty sure if the viscosity is too low it will just flow between the gaps. Finally, should I wax and release agent the moulds before casting ?
Thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fast Cast Polyurethane Casting Resin 2kg Pack
Jack.Strong
-
12 Years Ago
2.12 litres right ? :S
Jack.Strong
-
12 Years Ago
You will need to seal the join line so it can't leak out. Increasing the viscosity won't stop that...
Warren (Staff)
-
12 Years Ago
lol back to school for me :S Cheers
Jack.Strong
-
12 Years Ago
What you can do is fill the shape you want to cast with sugar or rice, then you remove all the rice...
matthieutje65
-
12 Years Ago
Or use water as long as you have time to let it dry properly. Less likely to leave dust on your...
Warren (Staff)
-
12 Years Ago
Lol as it being a 2 part mould I had trouble sealing the edges. So i silicone sealed it with my...
Jack.Strong
-
12 Years Ago
A hint for getting apart moulds when you use silicones is either slide a slim butter knife type...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search