Group: Administrators
Posts: 134,
Visits: 614
|
Hi Fabian,
Trust the chart on here, the Infusion PDF guide requires an update, as long as you are watching the infusion even is you mix too little resin you can effectivly 'pause' the infusion by clamping both feed and vacuum lines while you mix a bit more resin. But you are about spot-on with 250g so that's where I would start.
Paul Statham Easy Composites / Carbon Mods - Technical
|