Hey guyz,

can I use High Density Polyurethane Foam Block or extruded polystyrene to create a mould, then finish it for a clean and smooth surface, and then infuse my carbon parts on it? Or should I only use it for creating the pattern of my carbon part?

Thank you in advance!
MNM
MNM
Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)
Group: Forum Members
Posts: 6, Visits: 56
Anyone?
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K

In the video you can see they use PU-foam (pink) as mould for their Prepreg-parts....
So I guess its plausible 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Yep I do that quite a lot for "one offs" You will have to seal the foam with something like Epoxy Resin to give you a surface that you can polish. The reason I say for "one offs" is that the pattern usually gets destroyed when you demould.

Warren

Carbon Copies Ltd
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
The pink blocks are epoxy toolling block cnc milled. 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
No, The pink blocks are High density PU, use them all the time Smile strong as wood but no splinters and easy to sand the way you like it

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search