Hey guyz,

can I use High Density Polyurethane Foam Block or extruded polystyrene to create a mould, then finish it for a clean and smooth surface, and then infuse my carbon parts on it? Or should I only use it for creating the pattern of my carbon part?

Thank you in advance!
By matthieutje65 - 2/13/2013 2:39:41 AM

No, The pink blocks are High density PU, use them all the time Smile strong as wood but no splinters and easy to sand the way you like it