Hi 

I'm trying to make the front bumper of my honda civic ep3




The problem I have is that there are a number of layers it may need to be of adequate strength, and if you include some sort of core.

He planned to make a layer 200gr and 650gr a tending thickness of just over 1mm, with infusion




Let's see if I can lend a hand




thanks
Reply
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
I've made a front bumper for a rallycar and used 4 layers of material: CF 200gsm; Kevlar 300gsm; Kevlar 300gsm; CF 295gsm - that seems very strong although the shape & relatively small width (180mm) will help. 

Your bumper is more like a panel and if its a Type R bumper there is a fairly long thin run across the bottom, I'd expect to use some soric or extra layer on the large side areas and to p[rovide extra strength along the bottom.

Hope that helps
Stuart