Beginners' Guide to Out-of-Autoclave Prepreg Carbon Fibre


Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Everyone,

21 page tutorial guide with lots of detailed photographs throughout explaining the complete process from start to finish for simple out-of-autoclave prepreg carbon fibre. Available to download completely free using the link below.

This guide will accompany our new Prepreg Carbon Fibre Starter Kit and will of course be followed up with a video tutorial in the not too distant future.

Please provide any feedback on this tutorial here. If anything is unclear of could be explained better (or you spot any mistakes) then please let me know; I can use your input to improve the guide for everyone and ensure that the video tutorial is spot-on.

I look forward to hearing your thoughts and particularly to seeing your results if you follow this guide yourself.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Attachments
Replies
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Matt (Staff) (06/01/2013)
Hi Fred,

Fascinating stuff! - You're right that smaller vessels are available and if you can fit what you need to make into them then it can be more within reach (although maybe not so many people are as technically minded as yourself). When I think autoclave I tend to think of larger vessels (we have a 4m x 2m x 2m vessel, it weighs 7 tonnes!) but you're quite right that much smaller vessels are more widely available in the form of pressure pots or scientific autoclaves (often used for sterilizing).

We did have another customer who had built his own autoclave but I won't post any details of that in case I get sued.... It was not so legitimate as yours!

Still, anyone reading this article should keep in mind that the fastest growing area of prepreg is out-of-autoclave and I defy anyone to be able to tell the difference (we certainly couldn't).

--Matt


Hi Matt
I have heard that and I am very eager to try prepreg in and out of the autoclave. Is it possible to ship your special prepreg to Canada?
Fred

Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Fred, 

Yes, it's totally straight forward to send it anywhere in the world (prepreg does not count as 'dangerous goods').

Warren, Fred sounds like he knows what he's doing with this vessel. A purpose build pressure vessel will have been engineering with a good safety margin but like Fred points out, an autoclave is under pressure, it,s not a vacuum chamber. If it was, apart from being useless for prepreg, it would not really be any safety concern.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 13 Years Ago
     A good read :)
Jack.Strong - 13 Years Ago
Warren - 13 Years Ago
chihuahua46 - 13 Years Ago
matvd - 13 Years Ago
Matt (Staff) - 13 Years Ago
matthieutje65 - 13 Years Ago
Matt (Staff) - 13 Years Ago
                             thanks Matt, This makes everything clear! I'll give it a go soon
matthieutje65 - 13 Years Ago
Tim Ane - 6 Years Ago
alebassa - 13 Years Ago
Leon - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
Warren - 13 Years Ago
fgayford - 13 Years Ago
brasco - 13 Years Ago
fgayford - 13 Years Ago
Warren - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
Matt (Staff) - 13 Years Ago
mikew - 13 Years Ago
Element6 - 13 Years Ago
WilliamsHPF - 13 Years Ago
Matt (Staff) - 13 Years Ago
WilliamsHPF - 13 Years Ago
WilliamsHPF - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
Jack.Strong - 13 Years Ago
WilliamsHPF - 13 Years Ago
             Haha, OK, not a problem :)
Matt (Staff) - 13 Years Ago
matthieutje65 - 13 Years Ago
Matt (Staff) - 13 Years Ago
TomDesign - 13 Years Ago
Warren - 13 Years Ago
ajb100 - 13 Years Ago
Tim Ane - 6 Years Ago
Hanaldo - 6 Years Ago
Tim Ane - 6 Years Ago
                 debulk every couple layers and you should be fine
SleepingAwake - 6 Years Ago
Hanaldo - 6 Years Ago
Tim Ane - 6 Years Ago
Hanaldo - 6 Years Ago
raygun - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search