so i am here bored and watching youtube vids on fiberglass mold making.
this guy's vid ..well he seemed like a loud mouth blowhard LOL but he used a
kitchen mixer (for cake mix etc) to mix his resins.
i might have to try this-- thinking mix with mixer, then scrape sides and bottom of mix
 cup with wood mixing stick, mix some more then transfer to fresh paper cup with the
idea to as much as possible to avoid leaving any incomplete mixed resins in the cup.

do any of you use a mixer? or something in a cordless drill? handmixing for 5 minutes
get tedious so i am looking for a better faster way. does this add bubbles in the resins?
i think after  mixing i should put my resin mix in a vac chamber to de gas.

comments?

thanks everyone


scott    Smooooth


CarbonFiberCreations



Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Haven't tried a mechanical mixer but using a kitchen mixer would probably add a lot of air.

Mixing for 5 minutes sounds a lot to me. With epoxy you can see the swirls inside it and target getting them.