	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Generally the problem is the other way round, epoxy in polyester.  So you should be able to make a mould from epoxy and use it to make polyester parts.  If you are only making polyester parts then a traditional polyester based mould system would likely be a cheaper option. 
  The Uni-Mould System uses a Vinylester tooling Gelcoat which means it is fine to make epoxy, polyester and vinylester parts in a Uni-Mould tool.                
			            
  				