By FiveO - 9/13/2022 7:03:21 AM
Hi!
Can I make Epoxy tooling for casting polyester resin parts, or there are problems between these two? Can I make Epoxy tooling with UG1 Uni-Mould Tooling Gelcoat or I need to use Epoxy Tooling Gelcoat?
Thanks
|
By Warren (Staff) - 9/14/2022 9:54:02 AM
Uni-Mould is virtually zero shrinkage due to the fillers when compared to traditional polyester resins.
|
|