I'm new in the vacuum infusion so I have a few questions.
I want to make a composite part and for the female mold I'm gonna use a fire scale diam. 80 cm. depth 14 cm. I had the idea to make a box around in formica so I have a flange to attach the vacuum bag. Can you give me some advice about the position for installing the vacuum and infusion line. Do I place the infusion connector (with or without spiral tube) in the middle of the part or on the flange? For the vacuum line, is a connector enough or better in combination with a spiral tube?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hanaldo is spot on (as usual!).  Keeping the distance to a sensible level will help.  The shape is also a big factor in terms of where the resin is likely to flow.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant