Hi everyone. this might be a bit of a longshot but im just wondering, which manufacturer boasts the highest temperature resistance for their resin when cured. thanks
Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Highest outright I've seen is Sicomin SR1720/SD7840 with a service temperature of 200° C. That's obviously following a post cure, not a room temperature cure, as will be the case for all resins.

How big is the part you're making? I've had success infusing regular high temperature laminating epoxy (which is just about the consistency of honey at room temperature) by pre-heating it to 50° C before mixing. I wouldn't try anything too large with it though, the stuff I use has a pot-life at 25° of 90 minutes, and when heated to 50° that drops the pot-life down to about 15 minutes and it kicks extremely quickly if it sits in the pot not infusing quick enough. Mixing in batches means you can extend it a bit, but even the thin film in the part will gel pretty quickly so it would be pretty limited to parts under 1sqm.
Lester Populaire
L
Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
cole-P - 9/4/2021 8:38:19 PM
Hi everyone. this might be a bit of a longshot but im just wondering, which manufacturer boasts the highest temperature resistance for their resin when cured. thanks


Araldite® LY 8615 Resin with hardener Aradur® 8615 has a Tg of 217°C.