So Iv had 3 moulds stick on me now. I'm using tr108 wax as it's advertised to reduce fish eye when gel coat goes into the mould.

I have tried exact instructions on tin 8 coats and then leave over night before another coat.

Also tried 5 chem release followed by 2 tr108 wax.

I brush in polyester gel coat let dry. Lay up and  infuse with epoxy In2 resin and cure in mould at 60deg straight away for about 8 hours so it gels fast in the event of a leak.

The shiney parts of the mould released just about but everywhere else stuck like s***!

But should I be laying in a layer of fibreglass and pulling that out once cured to break in mould first?

Any help appreciated.
Edited 4 Years Ago by carbon man
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
When the new mould was made did it all cure really well? Gelocoat? and laminate? Correct temperatures etc?

Undercured cured moulds can often are recipe for a stickup regardless of release agents and application of them. 

https://www.rexco-usa.com/why-molds-stick/

I always use semi-permanent release agents and wax coats with wet layup moulds.







GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon man - 4 Years Ago
KLComposites - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
MarkMK - 4 Years Ago
carbon man - 4 Years Ago
MarkMK - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Fasta - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search