Frekote, Chemlease, Zyvax, Marbocote. Have a look for any of those. Not very familiar with American suppliers, but I know Soller Composites used to have Frekote 770NC and possibly still do, while Chemtrend are an American company and they make Chemlease and Zyvax over there, I know the Zyvax I buy here comes from an American plant.
|