After 3 fails its time to ask where i go wrong..


Author
Message
jeffrey bres
j
Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)Supreme Being (503 reputation)
Group: Forum Members
Posts: 42, Visits: 469
As mentioned..   3x not a charm here.

I have this isseu every time.
Clearcoating without gelcoat would be an option. But allso that isnt easy with small holes like this.

Now i used gelcoat. Hoping it would help.

Gel had cured at 25 degrees for 5 hours was dry to touch.

I used 3m high tack clear spray adheasive to hold the fibers in place. (AS LITTLE AS POSSIBLE)


on the vacuum catch pot the dail says my vacuum is 100%
I leace the pump running over night.  In the morning when the resin is hardned the vacuum line form the ez composite starter kit to the pot is flat from the vac. 

(I dont have an official cacuum pump.  I use a 35l/m fridge pump. Whitch seems to work fine.   I can add an extra pump if i need more cfm...)
If my vac is to strong.. i can make a bleedvalve to reduce vacuum.   

But idialy i would love to have a perfect finish.

I use easy lease release agent..  denoulding is a breeze..




Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
As you are likely talking about plate stiffness the best solution might be a foam core glass or carbon laminate. This leaves the option to switch to solid glass at some places.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago
explorecomposites - 4 Years Ago
jeffrey bres - 4 Years Ago
jeffrey bres - 4 Years Ago
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
Warren (Staff) - 4 Years Ago
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
Warren (Staff) - 4 Years Ago
jeffrey bres - 4 Years Ago
explorecomposites - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago
mporta71 - 4 Years Ago
                 Mostly damage tolerance
SleepingAwake - 4 Years Ago
jeffrey bres - 4 Years Ago
oekmont - 4 Years Ago
jeffrey bres - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago
oekmont - 4 Years Ago
Hanaldo - 4 Years Ago
jeffrey bres - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search