	Group: Forum Members 	        
    Posts: 2.5K, 
    Visits: 28K 
    
 
          
		     | 
				                       
                 
                
                    
			            There are a few strange things going on here, but the drilling that hole and sticking your fitting through it is the one that stands out to me. I would suggest watching the Easy Composites infusion tutorial videos and following those setups more closely to avoid issues.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |