Carbon Fiber Plate - 2 Side Glossy Finish


Author
Message
Frizou
F
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 3, Visits: 9
Hello to all!

I'm new to composites and diving in!

I would like your suggestion on making 2 sided glossy GF plates. 1mm to 6 mm

I did start a test of infusion in between 2 glass panels that are waxed. Am I off track oy not?

What do production shops do?

Thanks
Reply
Frizou
F
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 3, Visits: 9
Chris Rogers - 10/23/2020 12:53:22 AM
The glass plates method seems to work ok for small things but it doesn't do much to control the thickness in a uniform way - and the glass is scary to handle routinely.  The gold standard for plate making is a large heated press which will keep the pressure even - and prepreg. 

For infusion, you can use a caul plate (what one sheet of your glass is) and a shiny mold (the other sheet) but your flow distance will be limited to a meter (in ideal conditions) without core - and even then you may end up with slightly tapered plates from edge to edge.  If you can bury some inter-laminar flow media like G-flow in there or get a fabric with a micro web ply to help with flow you may have better luck too... but at a cost to plate performance.  

How big do you need and what are you using them for?

Well I'm in a learning phase and the size of my plates are small (starting at 24''x24'' or 635mm X 635mm). For the moment I want to start with infusion and go from there! Are their some manufacturer or youtube I can look at to gather more info on heated press for the future.