Group: Forum Members
Posts: 54,
Visits: 250
|
Prepregs, no other way. I have tried a plates made of polished aluminium sheets thk of 12mm instead glass, vacuumed, pressed in autoclave +8bar, baked. The result was great, but needs a lot of experience and technology. The 2-shot process like Hanaldo talking about is quite OK, but you have to bond it together in jig plates as well to keep constant thickness.
|