What type of cloth is this


Author
Message
Mrcirrus
M
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 19
LOL I’ve just realised your Warren from easy composites who sold me the plain weave in the first place and told me it was a match !!! Didn’t realise this was Easy composites forum, no worries, very happy with the service your company provides, keep up the good work.
Mrcirrus
M
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 19
Yes I’ve just checked and it’s 90GSM I’ve got. I’ve a sample of 210GSM but that’s 5 tows per cm. Pinarello state Toray T1100 1k but that might be the unidirectional which sits underneath the weave. Thanks for the reply anyway. Makes me wonder what these pro bike repairs use?


Warren (Staff)
Warren (Staff)
Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)Supreme Being (15K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8K
There are some slightly heavier Plain Weave's around but they are really rare.  We used to stock a 130g plain weave which was actually really nice as compared to the 90g the pattern was much denser and less gappy.  Unfortunately the manufacturer stopped making it as otherwise I'd be pointing you in that direction!

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Mrcirrus
M
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 19
I want to identify some carbon cloth. I’m repairing a carbon bike, Pinarello f8. The carbon is visible under clear coat so I’m after the exact same weave. I ordered some 1k plain weave but it’s not quite the same because it’s a loose weave (I can see lots of holes Holding up to the light). This looks like a very square and dense pattern, almost like spread toe. It’s about 7 picks percm and approx .2mm thick. Can anybody identify it? Picture below.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search