Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
What type of cloth is this
What type of cloth is this
Post Reply
Like
7
What type of cloth is this
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Mrcirrus
M
Mrcirrus
posted 6 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 3,
Visits: 19
I want to identify some carbon cloth. I’m repairing a carbon bike, Pinarello f8. The carbon is visible under clear coat so I’m after the exact same weave. I ordered some 1k plain weave but it’s not quite the same because it’s a loose weave (I can see lots of holes Holding up to the light). This looks like a very square and dense pattern, almost like spread toe. It’s about 7 picks percm and approx .2mm thick. Can anybody identify it? Picture below.
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
What type of cloth is this
Mrcirrus
-
6 Years Ago
There are some slightly heavier Plain Weave's around but they are really rare. We used to stock a 130g plain weave which was actually really nice as compared to the 90g the pattern was much denser an...
Warren (Staff)
-
6 Years Ago
Yes I’ve just checked and it’s 90GSM I’ve got. I’ve a sample of 210GSM but that’s 5 tows per cm. Pinarello state Toray T1100 1k but that might be the unidirectional which sits underneath the weave......
Mrcirrus
-
6 Years Ago
LOL I’ve just realised your Warren from easy composites who sold me the plain weave in the first place and told me it was a match !!! Didn’t realise this was Easy composites forum, no worries, very.....
Mrcirrus
-
6 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search