Hi gents, I have been using different techniques during my time Carbon skinning to bond the cloth onto my parts.

The most convenient way I have found is using a spray adhesive to bond the cloth to the part then when dry, add my layers of XCR resin. My finish has been great and my parts seem to come out perfect. My main concern at the moment is the longevity of the bond.. is delamination something I should be worried about? Especially on exterior car parts?

I've not had any issues as of yet but delamination doesn't happen right away anyway.

Thanks you in advance!
Reply
Fastskiguy
F
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 11, Visits: 18
LukeSGee - 10/5/2020 7:26:49 PM
Hi gents, I have been using different techniques during my time Carbon skinning to bond the cloth onto my parts.

The most convenient way I have found is using a spray adhesive to bond the cloth to the part then when dry, add my layers of XCR resin. My finish has been great and my parts seem to come out perfect. My main concern at the moment is the longevity of the bond.. is delamination something I should be worried about? Especially on exterior car parts?

I've not had any issues as of yet but delamination doesn't happen right away anyway.

Thanks you in advance!

Sorry I can't help with your delamination questions but what type of adhesive are you using? Thanks Smile

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search