We wander if the carbon sheet prepp is effected by cutting fluids? normal Water solub, standard machine fluid, or a Shell Fenella VD 201 N?
We are trying to reduce particles and heat when cutting 1.5mm sheet or 2mm sheet with small tools 0.8mm and up to 4mm.
We don't want it to delaminate!!!!!!
Regards
Rob Mullins
Paul (Staff)
Paul (Staff)
Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)Technical Support (2.2K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Rob,

Normal cutting fluids will not harm the carbon laminate, oils and solvents can be an issue as they can penetrate the edge slightly so avoid these, once the components have been milled you should rinse them is fresh water and then dry them off, you should be fine to go ahead!

Paul Statham
Easy Composites / Carbon Mods - Technical
Joe
Joe
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi, Rob,

Dunno if it makes any sense with composites... But I had good results on aluminum milling with a permanent mist of ethanol. It would evaporate in a matter of seconds and leave a clean dry part.

I know some resins will blemish by the permanent contact of ethanol. But what about that mist during machining only? Before trying it, you might want the EC guys give their input.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search