Semi-permanent release agent vs wax


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi,
what are the scenarios where is better to use a semi permanent release agent and the ones where is better a wax?
Replies
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Fasta - 10/5/2020 5:50:32 AM
It's not always one or the other.

I use semi permenant release agents on all my moulds including the ones I want to use wax with. Semi perm and then wax on top too.

Thanks!
Why you add wax on top of semi permanent?

Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Massimiliano - 10/5/2020 5:58:15 AM
Fasta - 10/5/2020 5:50:32 AM
It's not always one or the other.

I use semi permenant release agents on all my moulds including the ones I want to use wax with. Semi perm and then wax on top too.

Thanks!
Why you add wax on top of semi permanent?

The semi permenant gives the mould a safer release and the wax allows you to spray gel coats on to the surface as well as making for a better gloss mould finish. I use this on moulds requiring wet resin layup and I use only semi permenant when working with pre preg and oven cure cooking.





Edited 5 Years Ago by Fasta
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Fasta - 10/5/2020 6:03:45 AM
Massimiliano - 10/5/2020 5:58:15 AM
Fasta - 10/5/2020 5:50:32 AM
It's not always one or the other.

I use semi permenant release agents on all my moulds including the ones I want to use wax with. Semi perm and then wax on top too.

Thanks!
Why you add wax on top of semi permanent?

The semi permenant gives the mould a safer release and the wax allows you to spray gel coats on to the surface as well as making for a better gloss mould finish. I use this on moulds requiring wet resin layup and I use only semi permenant when working with pre preg and oven cure cooking.

Understood, thank you!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
             Thank you
mporta71 - 5 Years Ago
Fasta - 5 Years Ago
mporta71 - 5 Years Ago
Fasta - 5 Years Ago
                     Understood, thank you!
mporta71 - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you for the additional advice
mporta71 - 5 Years Ago
chriscnf - 5 Years Ago
Fasta - 5 Years Ago
chriscnf - 5 Years Ago
Fasta - 5 Years Ago
                             Thanks...appreciate you help and this forum...brilliant
chriscnf - 5 Years Ago
carguy84 - 4 Years Ago
Hanaldo - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search