+x Massimiliano - 10/5/2020 3:45:35 AMHi,what are the scenarios where is better to use a semi permanent release agent and the ones where is better a wax?
+x Lester Populaire - 10/5/2020 5:12:20 AM+x Massimiliano - 10/5/2020 3:45:35 AMHi,what are the scenarios where is better to use a semi permanent release agent and the ones where is better a wax?I use wax for surfaces that have some level of porosity (like body filler) and surfaces that are not resistant to solvents. Usually permanent releases for everything else even tho we started using formula five wax for more and more things to reduce exposure to solvents.