Rubbing strip oldtimer problems
Rubbing strip oldtimer problems
Post Reply
Like
6
Rubbing strip oldtimer problems
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
dubster
dubster
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 15,
Visits: 126
Hi guys,
I had a few experiments to cast a rubbing strip for oldtimer bumpers (middle of the bumper). So these cars aren't outside for months, but strip needs to be sort of weather proof
So I bended a aluminium for mould, shape is perfect.
After using some casting rubbers (including UV stabilisator) I keep having strange complications.
UV really kicks in after 14 days:
strange spots after rain:
color fading away after 14 days
is there someone who can point me to the right (easy comp) kind of product? needs to be a little flexible / soft ...
thanks in advance !!
Reply
Like
6
Reply
dubster
dubster
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 126
UR 3450 Sika
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Rubbing strip oldtimer problems
dubster
-
6 Years Ago
You really need a UV stable resin by the looks of it. Certainly a strange reaction there. I would expect fading or maybe some kind of surface degradation but that is quite unusual. Are you sure the.....
Warren (Staff)
-
6 Years Ago
ok, might make another one and let these one cure longer? the resin was 24H in the mould like asked (the pix are 2 different resins). after that I left it outside for a few weeks. looks mint when...
dubster
-
6 Years Ago
hi what is your resin?
ana
-
6 Years Ago
If it is not fully cured, it will still be hydroscopic. 24 hours may be fine for demould but, like most resin systems, the tail end of the resin cure may be longer. I would leave it a good week to...
Warren (Staff)
-
6 Years Ago
ok, thanks for the advice Warren. is there a easycomp resin - product that suits the specs i need?
dubster
-
6 Years Ago
Our flexible PU's are not 100% UV stable so you may still suffer from pigment fade over time.
Warren (Staff)
-
6 Years Ago
UR 3450 Sika
dubster
-
6 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search