That part looks fantastic in shape and design, well done getting it replicate to that result
I think you did not polish the wax off fully or may have used release agent on top of that wax, coating it with spray adhesive etc. Don't be offended that is just a thought and I may be wrong
I use release agent only now on moulds made from epoxy or polyester having had lots of problems applying over-callously layers of wax or PVA on top of that all the best and good luck
|