Maximun fabric thickness for infusion


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, what is the recommended maximum fabric thickness for a one shot successful infusion, given a 250 cm2 square area?
Thanks


Edited 5 Years Ago by Massimiliano
Replies
Rosta Spicl
Rosta Spicl
Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)Supreme Being (574 reputation)
Group: Forum Members
Posts: 54, Visits: 250
See the waffle. That's generally a pan, supported by lattice structure from the bottom side - it means bottom area of pan filled by crossing ribs fixed to the side flanges of pan. Understand?
Remember, from the rigidity point of view the height of ribs is the much more important than rib width.

Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Rosta Spicl - 9/9/2020 11:52:45 AM
See the waffle. That's generally a pan, supported by lattice structure from the bottom side - it means bottom area of pan filled by crossing ribs fixed to the side flanges of pan. Understand?
Remember, from the rigidity point of view the height of ribs is the much more important than rib width.

Thank you, understand!
You got me hungry too :-)


Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Massimiliano - 9/9/2020 12:01:26 PM
Rosta Spicl - 9/9/2020 11:52:45 AM
See the waffle. That's generally a pan, supported by lattice structure from the bottom side - it means bottom area of pan filled by crossing ribs fixed to the side flanges of pan. Understand?
Remember, from the rigidity point of view the height of ribs is the much more important than rib width.

Thank you, understand!
You got me hungry too :-)


Can anyone recommend number of layers and carbon fiber type(s) to achieve the 2mm thickness?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
mporta71 - 5 Years Ago
DD-Compound - 5 Years Ago
explorecomposites - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
DD-Compound - 5 Years Ago
explorecomposites - 5 Years Ago
mporta71 - 5 Years Ago
Rosta Spicl - 5 Years Ago
Rosta Spicl - 5 Years Ago
mporta71 - 5 Years Ago
Rosta Spicl - 5 Years Ago
mporta71 - 5 Years Ago
mporta71 - 5 Years Ago
DD-Compound - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
                     Thank you, will do as you suggest!
mporta71 - 5 Years Ago
DD-Compound - 5 Years Ago
DD-Compound - 5 Years Ago