I have made some new fuel tank floats out of cork for a vintage vehicle. They need proofing against 100 low lead octane fuel. Can you please recommend a suitable product? In the old days, they were coated with shellac, but having tried and failed I'm now looking for a suitable resin. Thanks.
Reply
Dave Reid
D
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 13
Hanaldo - 8/4/2020 1:35:18 PM
Phenol novolac epoxy is the go. 

Thanks both - I'll give it a try!