Hi all, just looking for some advice please,
I have a motorsport wing for my Exige that is looking rather tired on top. The fibres appear to be completely dry in sections but thankfully no damage. I have been told that the wing has been previously clear coated by the previous owner, but i would rather use something like the XCR kit to properly protect the fibres underneath. With the local areas of exposed carbon I am very nervous about sanding down too much, if there is some lacquer left in areas will this cause problems with laying down new epoxy from the XCR kit?