Hi all, just looking for some advice please, 

I have a motorsport wing for my Exige that is looking rather tired on top. The fibres appear to be completely dry in sections but thankfully no damage. I have been told that the wing has been previously clear coated by the previous owner, but i would rather use something like the XCR kit to properly protect the fibres underneath.
With the local areas of exposed carbon I am very nervous about sanding down too much, if there is some lacquer left in areas will this cause problems with laying down new epoxy from the XCR kit?


Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search