Alternatives to carbon fiber and resin for testing setups as a dry run


Alternatives to carbon fiber and resin for testing setups as a dry run
Author
Message
Barry Marsh
Barry Marsh
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 19, Visits: 65
Hi,

Was wondering if anybody has any good suggestions to alternatives to carbon fiber and resin for testing setups. So that I am not wasting as much carbon and resin I am looking for a way to do a dry run.

I had thought maybe some kind of cheap material and a liquid that has a similar viscosity to the IN2 resin that EC sells.

I understand that the only real way to test is with the real materials but wonder if there would be any value in doing a test like this and if anybody on here does this?

Thanks for any input / ideas
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh just use fibreglass and perhaps an infusion polyester for a cheap resin. The only downside is polyester/vinyl esters infuse slightly differently to epoxies, but they are certainly close enough to just get the hang of the process. 
Barry Marsh
Barry Marsh
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 19, Visits: 65
Yeah thanks again the the extra suggestion there. I didn’t so much need anything that would set, but just to get an idea about the flow while it’s live.